The XRD analysis of the prepared sample of TiO 2 nanoparticles was done using a Bruker make diffractometer, Cu-Kα X-rays of wavelength (λ)=1.5406 Å and data was taken for the 2 θ range of 10° to 70° with a step of 0.1972°.
Titanium oxide (TiO2) nanoparticles were fabricated using the sol-gel technique. By controlling the calcination temperature, the different structures of TiO2 (anatase and rutile) have been...
1 Ιουλ 2013 · Morphology index (MI) derived from FWHM of XRD data explains the interrelationship of particle size and specific surface area. It is observed that MI has direct relationship with particle size...
The surface structure observed via FESEM images reveals that different current densities yield different nanotubular TiO2 structures, predominantly in the form of anatase TiO2 crystals.
In this study, the commercial TiO2 nanopowder and micropowder of anatase phase and rutile phase have been characterized by x-ray diffraction (XRD) and transmission electron microscopy (TEM). XRD patterns of nano-TiO2 in rutile and anatase phases exhibit broad peaks whereas both phases of micro-TiO2 demonstrate very sharp peaks.
23 Ιουλ 2019 · X-ray diffraction (XRD) patterns for samples of nanoparticles having different sizes and shapes can look different, and careful analysis of the XRD data can provide useful information and also help correlate microscopic observations with the bulk sample.
1 Ιουλ 2022 · Abstract. For more than 20 years, Pt/TiO 2 represents the benchmark photocatalyst/co-catalyst platform for photocatalytic hydrogen (H 2) generation. Here, single atom (SA) Pt is decorated on different polymorphs of TiO 2 (anatase, rutile, and the mixed phase of P25) using a simple immersion anchoring approach.